Angelim vs Angelim-pedra

Hymenolobium sp against Hymenolobium petraeum. Every number below names the publication it came from.

PropertyAngelimAngelim-pedra
Janka hardness1,422 lbfLPF/SFB Madeiras Brasileiras1,301 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC44.9 lb/ft³LPF/SFB Madeiras Brasileiras44.3 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture16,228 lb/in²LPF/SFB Madeiras Brasileiras15,858 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.72 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.68 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength8,164 lb/in²LPF/SFB Madeiras Brasileiras7,581 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)9.9%LPF/SFB Madeiras Brasileiras10.1%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.95LPF/SFB Madeiras Brasileiras1.54LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.