Compare two woods
Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.
Angelim-amargoso vs Faveira-amargosa
Vatairea sericea against Vatairea paraensis. Every number below names the publication it came from.
| Property | Angelim-amargoso | Faveira-amargosa |
|---|---|---|
| Janka hardness | 2,167 lbfLPF/SFB Madeiras Brasileiras | 2,174 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 56.2 lb/ft³LPF/SFB Madeiras Brasileiras | 62.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 19,323 lb/in²LPF/SFB Madeiras Brasileiras | 21,519 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.15 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.18 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 10,525 lb/in²LPF/SFB Madeiras Brasileiras | 11,280 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 13.9%LPF/SFB Madeiras Brasileiras | 14.0%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.87LPF/SFB Madeiras Brasileiras | 2.04LPF/SFB Madeiras Brasileiras |
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.
Published comparisons
400 selected pairs, each with a published Janka test for both woods.
- Urucurana vs Urucurana
- Miraúba vs Urucurana
- Urucurana vs Urucurana
- Curupay vs Urucurana
- Jatobá / jutaí-do-campo vs Urucurana
- Urucurana vs Wamara
- Miraúba vs Urucurana
- Urucurana vs Urucurana
- Curupay vs Urucurana
- Jatobá / jutaí-do-campo vs Urucurana
- Urucurana vs Wamara
- Curupay vs Miraúba
- Jatobá / jutaí-do-campo vs Miraúba
- Miraúba vs Wamara
- Ipe vs Miraúba
- Curupay vs Jatobá / jutaí-do-campo
- Curupay vs Wamara
- Curupay vs Ipe
- Curupay vs Jataipeba
- Jatobá / jutaí-do-campo vs Wamara
- Ipe vs Jatobá / jutaí-do-campo
- Jataipeba vs Jatobá / jutaí-do-campo
- Jatobá / jutaí-do-campo vs Marishballi
- Ipe vs Wamara
- Jataipeba vs Wamara
- Marishballi vs Wamara
- Jarana vs Wamara
- Ipe vs Jataipeba
- Ipe vs Marishballi
- Ipe vs Jarana
- Jataipeba vs Marishballi
- Jarana vs Jataipeba
- Jataipeba vs Manbarklak
- Jarana vs Marishballi
- Manbarklak vs Marishballi
- Marishballi vs Muirapixuna
- Jarana vs Manbarklak
- Jarana vs Muirapixuna
- Cumaru vs Jarana
- Jarana vs Rosadinho
- Casca-preciosa vs Jarana
- Manbarklak vs Muirapixuna
- Cumaru vs Manbarklak
- Manbarklak vs Rosadinho
- Casca-preciosa vs Manbarklak
- Cumaru vs Muirapixuna
- Muirapixuna vs Rosadinho
- Casca-preciosa vs Muirapixuna
- Maria-preta vs Muirapixuna
- Cumaru vs Rosadinho
- Casca-preciosa vs Cumaru
- Cumaru vs Maria-preta
- Casca-preciosa vs Rosadinho
- Maria-preta vs Rosadinho
- Caraiperana vs Rosadinho
- Casca-preciosa vs Maria-preta
- Caraiperana vs Casca-preciosa
- Casca-preciosa vs Pau-santo
- African ebony vs Azobe
- Azobe vs Casca-preciosa
- Azobe vs Maria-preta
- Azobe vs Rosadinho
- Azobe vs Rhodesian-Teak
- Azobe vs Caraiperana
- Caraiperana vs Maria-preta
- Maria-preta vs Pau-santo
- Maçaranduba vs Maria-preta
- Caraiperana vs Pau-santo
- Caraiperana vs Maçaranduba
- Caraiperana vs Castanha-de-cutia
- Maçaranduba vs Pau-santo
- Castanha-de-cutia vs Pau-santo
- Bulletwood vs Pau-santo
- Angelim / angelim-rajado vs Pau-santo
- Maçaranduba vs Maçaranduba
- Castanha-de-cutia vs Maçaranduba
- Bulletwood vs Maçaranduba
- Angelim / angelim-rajado vs Maçaranduba
- African ebony vs East African Olive
- African Celtis vs African ebony
- African ebony vs East African Camphorwood
- African ebony vs African mahogany
- African Canaríum vs African ebony
- Castanha-de-cutia vs Castanha-de-cutia
- Bulletwood vs Castanha-de-cutia
- Angelim / angelim-rajado vs Castanha-de-cutia
- Castanha-de-cutia vs Pracuúba-da-terra-firme
- Castanha-de-cutia vs Macucu-branco
- Brush Box vs Casuarina
- Castanha-de-cutia vs Casuarina
- Bulletwood vs Casuarina
- African ebony vs Casuarina
- Angelim / angelim-rajado vs Casuarina
- Casuarina vs Maçaranduba
- Angelim / angelim-rajado vs Bulletwood
- Bulletwood vs Pracuúba-da-terra-firme
- Bulletwood vs Macucu-branco
- Bulletwood vs Macawood
- Angelim / angelim-rajado vs Pracuúba-da-terra-firme
- Angelim / angelim-rajado vs Macucu-branco
- Angelim / angelim-rajado vs Macawood
- Angelim / angelim-rajado vs Cachaporra-do-gentio
- East Indian Satinwood vs Indian rosewood
- Brazilian rosewood vs Indian rosewood
- Belian vs Indian rosewood
- Indian Laurel vs Indian rosewood
- East Indian ebony vs Indian rosewood
- Gangaw vs Indian rosewood
- Macucu-branco vs Pracuúba-da-terra-firme
- Macawood vs Pracuúba-da-terra-firme
- Cachaporra-do-gentio vs Pracuúba-da-terra-firme
- Macawood vs Macucu-branco
- Cachaporra-do-gentio vs Macucu-branco
- Cachaporra-do-gentio vs Macawood
- Ipê vs Macawood
- Cachaporra-do-gentio vs Ipê
- Cachaporra-do-gentio vs Sapucaia
- Ipê vs Sapucaia
- Cabreúva-parda vs Ipê
- Ingá vs Ipê
- Ipê vs Macucu-branco
- Sapucaia vs Sapucaia / sapucaia-vermelha
- Cabreúva-parda vs Sapucaia
- Ingá vs Sapucaia
- Macawood vs Sapucaia
- Brush Box vs Ipê
- Brush Box vs Sapucaia
- Brush Box vs Cabreúva-parda
- Brush Box vs Turpentine
- Brush Box vs Ingá
- Cabreúva-parda vs Ingá
- Cabreúva-parda vs Maçaranduba
- Angelim-vermelho vs Cabreúva-parda
- Cabreúva-parda vs Mururé
- Ingá vs Ingá
- Ingá vs Maçaranduba
- Angelim-vermelho vs Ingá
- Ingá vs Mururé
- Angelim-vermelho vs Maçaranduba
- Maçaranduba vs Mururé
- Ipê vs Maçaranduba
- Angelim-vermelho vs Mururé
- Angelim-vermelho vs Ipê
- Angelim-vermelho vs Sapucaia
- Ipê vs Mururé
- Mururé vs Sapucaia
- Belian vs Gangaw
- Belian vs Mururé
- Angelim-vermelho vs Belian
- Belian vs Maçaranduba
- Belian vs Rhodesian-Teak
- Muhimbi vs Rhodesian-Teak
- Missanda vs Rhodesian-Teak
- Okan vs Rhodesian-Teak
- African ebony vs Rhodesian-Teak
- East African Olive vs Rhodesian-Teak
- Kamassi vs Rhodesian-Teak
- Missanda vs Muhimbi
- Muhimbi vs Okan
- East African Olive vs Muhimbi
- African ebony vs Muhimbi
- Kamassi vs Muhimbi
- Abiurana vs Aromata
- Aromata vs Uxirana
- Abiurana-seca vs Aromata
- Angico vs Aromata
- Aromata vs Tuturubá
- Abiurana vs Aromata
- Abiurana vs Abiurana
- Abiurana vs Abiurana
- Abiurana vs Abiurana
- Abiurana vs Uxirana
- Abiurana vs Abiurana-seca
- Abiurana vs Angico
- Abiurana-seca vs Uxirana
- Angico vs Uxirana
- Tuturubá vs Uxirana
- Abiurana vs Uxirana
- Abiurana-seca vs Angico
- Abiurana-seca vs Tuturubá
- Abiurana vs Abiurana-seca
- Angico vs Tuturubá
- Abiurana vs Angico
- Missanda vs Okan
- East African Olive vs Missanda
- Kamassi vs Missanda
- Bubinga vs Missanda
- Tuturubá vs Tuturubá
- Abiurana vs Tuturubá
- Sucupira vs Tuturubá
- Kaneelhart vs Tuturubá
- Abiurana vs Abiurana
- Abiurana vs Abiurana
- Abiurana vs Sucupira
- Kaneelhart vs Sucupira
- Angico vs Sucupira
- Abiurana-seca vs Sucupira
- Sucupira vs Sucupira
- Abiurana vs Kaneelhart
- Angico vs Kaneelhart
- Abiurana-seca vs Kaneelhart
- Kaneelhart vs Uxirana
- East Indian Satinwood vs Gangaw
- Gangaw vs Kaneelhart
- Gangaw vs Sucupira
- Abiurana vs Gangaw
- Ingá vs Sapucaia / sapucaia-vermelha
- Ingá vs Tanimbuca
- Ingá vs Kaneelhart
- Ingá vs Sucupira
- Abiurana vs Ingá
- Sapucaia / sapucaia-vermelha vs Tanimbuca
- Kaneelhart vs Sapucaia / sapucaia-vermelha
- Sapucaia / sapucaia-vermelha vs Sucupira
- Caraipé vs Sapucaia / sapucaia-vermelha
- Tanimbuca vs Tanimbuca
- Kaneelhart vs Tanimbuca
- Sucupira vs Tanimbuca
- Caraipé vs Tanimbuca
- East African Olive vs Okan
- Kamassi vs Okan
- Bubinga vs Okan
- Caraipé vs Maçarandubarana
- Brazilian rosewood vs Caraipé
- Black Cabbage-Bark vs Caraipé
- Caraipé vs Leche Perra
- Caraipé vs Castanha-de-cutia
- Barrote vs Caraipé
- Caraipé vs Turpentine
- East African Olive vs Turpentine
- Kamassi vs Turpentine
- Maçarandubarana vs Turpentine
- Okan vs Turpentine
- East African Olive vs East Indian Satinwood
- East African Olive vs Kamassi
- Bubinga vs East African Olive
- African Celtis vs East African Olive
- Bubinga vs Kamassi
- Kamassi vs Mecrusse
- Brazilian rosewood vs Maçarandubarana
- Black Cabbage-Bark vs Maçarandubarana
- Leche Perra vs Maçarandubarana
- Castanha-de-cutia vs Maçarandubarana
- Barrote vs Maçarandubarana
- Black Cabbage-Bark vs Brazilian rosewood
- Brazilian rosewood vs Leche Perra
- Brazilian rosewood vs Castanha-de-cutia
- Barrote vs Brazilian rosewood
- Black Cabbage-Bark vs Leche Perra
- Black Cabbage-Bark vs Castanha-de-cutia
- Barrote vs Black Cabbage-Bark
- Anoerá-ferro vs Black Cabbage-Bark
- Castanha-de-cutia vs Leche Perra
- Barrote vs Leche Perra
- Anoerá-ferro vs Leche Perra
- Barrote vs Castanha-de-cutia
- Anoerá-ferro vs Castanha-de-cutia
- Anoerá-ferro vs Barrote
- Bubinga vs Mecrusse
- Bubinga vs Muhimbi
- Anoerá-ferro vs Brazilian rosewood
- Anoerá-ferro vs Goiabão
- Abiurana-branca vs Goiabão
- Barrote vs Goiabão
- Castanha-de-cutia vs Goiabão
- Black Cabbage-Bark vs Goiabão
- Goiabão vs Leche Perra
- Abiurana-branca vs Anoerá-ferro
- Abiurana-branca vs Barrote
- Abiurana-branca vs Parinari / bafo-de-boi-mirim
- Abiurana-branca vs Castanha-de-cutia
- Abiurana-branca vs Pau-branco
- East Indian Satinwood vs Indian Laurel
- East Indian ebony vs East Indian Satinwood
- Abiurana-branca vs East Indian Satinwood
- East African Olive vs Mecrusse
- Mecrusse vs Okan
- Mecrusse vs Parinari / bafo-de-boi-mirim
- Mecrusse vs Pau-branco
- Parinari / bafo-de-boi-mirim vs Pau-branco
- Cuiarana vs Parinari / bafo-de-boi-mirim
- Canafístula vs Parinari / bafo-de-boi-mirim
- Oak vs Parinari / bafo-de-boi-mirim
- Abiurana vs Parinari / bafo-de-boi-mirim
- Parinari / bafo-de-boi-mirim vs Urucurana
- Cuiarana vs Pau-branco
- Canafístula vs Pau-branco
- Oak vs Pau-branco
- Abiurana vs Pau-branco
- Pau-branco vs Urucurana
- Canafístula vs Cuiarana
- Cuiarana vs Oak
- Abiurana vs Cuiarana
- Cuiarana vs Urucurana
- Canafístula vs Oak
- Abiurana vs Canafístula
- Canafístula vs Urucurana
- Abiurana vs Oak
- Oak vs Urucurana
- Abiurana vs Abiurana
- Abiurana vs Urucurana
- Abiurana vs Matamatá
- Matamatá vs Urucurana
- Matamatá vs Matamatá
- Matamatá vs Matamatá / sapucaia-amargosa
- Matamatá vs Matamatá
- Canafístula vs Matamatá
- Abiurana vs Matamatá
- Abiurana vs Tuturubá
- Abiurana vs Amora / amoreira
- Matamatá vs Matamatá / sapucaia-amargosa
- Matamatá vs Matamatá
- Matamatá vs Tuturubá
- Amora / amoreira vs Matamatá
- Amora / amoreira vs Tuturubá
- Fustic vs Tuturubá
- Demerara Greenheart vs Tuturubá
- Amora / amoreira vs Fustic
- Amora / amoreira vs Demerara Greenheart
- Amora / amoreira vs Courbaril
- Demerara Greenheart vs Fustic
- Fustic vs Matamatá
- Courbaril vs Fustic
- Fustic vs Greenheart
- Demerara Greenheart vs Greenheart
- Courbaril vs Demerara Greenheart
- Demerara Greenheart vs Fava-orelha-de-negro
- Demerara Greenheart vs Matamatá / sapucaia-amargosa
- Courbaril vs Greenheart
- Courbaril vs Fava-orelha-de-negro
- Courbaril vs Matamatá / sapucaia-amargosa
- Courbaril vs Uxi
- Fava-orelha-de-negro vs Greenheart
- Greenheart vs Matamatá / sapucaia-amargosa
- Greenheart vs Uxi
- Fava-orelha-de-negro vs Matamatá / sapucaia-amargosa
- Fava-orelha-de-negro vs Uxi
- Breu vs Fava-orelha-de-negro
- Matamatá vs Matamatá / sapucaia-amargosa
- Matamatá / sapucaia-amargosa vs Uxi
- Breu vs Uxi
- Demerara Greenheart vs Uxi
- Breu vs Mora
- Breu vs Matamatá / sapucaia-amargosa
- Breu vs Courbaril
- Breu vs Greenheart
- Mora vs Uxi
- Matamatá / sapucaia-amargosa vs Mora
- Fava-orelha-de-negro vs Mora
- Courbaril vs Mora
- Greenheart vs Mora
- Burma Lancewood vs Burma Padauk
- Burma Lancewood vs Pyinkado
- Burma Lancewood vs Indian Laurel
- Burma Lancewood vs Chengal
- Burma Lancewood vs Tembusu
- Burma Lancewood vs Ohia
- Indian Laurel vs Pyinkado
- Burma Padauk vs Pyinkado
- Chengal vs Pyinkado
- Pyinkado vs Tembusu
- Ohia vs Pyinkado
- Carne D'Anta vs Tanimbuca
- Balsamo vs Carne D'Anta
- Carne D'Anta vs Taniboca
- Carne D'Anta vs Mora
- Carne D'Anta vs Faveira-amargosa
- Breu-manga vs Carne D'Anta
- Tanimbuca vs Tanimbuca
- Balsamo vs Tanimbuca
- Taniboca vs Tanimbuca
- Faveira-amargosa vs Tanimbuca
- East Indian ebony vs Indian Laurel
- Burma Padauk vs Indian Laurel
- Chengal vs Indian Laurel
- Balsamo vs Taniboca
- Balsamo vs Faveira-amargosa
- Balsamo vs Breu-manga
- Balsamo vs Louro-faia
- Balsamo vs Pau-amarelo
- Angelim-amargoso vs Balsamo
- Faveira-amargosa vs Taniboca
- Breu-manga vs Taniboca
- Louro-faia vs Taniboca
- Pau-amarelo vs Taniboca
- Angelim-amargoso vs Taniboca
- Muhuhu vs Taniboca
- Balsamo vs Muhuhu
- Faveira-amargosa vs Muhuhu
- Burma Padauk vs Muhuhu
- Breu-manga vs Muhuhu
- Louro-faia vs Muhuhu
- Faveira-amargosa vs Faveira-amargosa
- Breu-manga vs Faveira-amargosa
- Faveira-amargosa vs Louro-faia
- Faveira-amargosa vs Pau-amarelo
- Angelim-amargoso vs Faveira-amargosa
- Faveira-amargosa vs Mandioqueira
- Burma Padauk vs Chengal
- Burma Padauk vs Tembusu