Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Angelim-pedra vs Para-angelim

Hymenolobium modestum against Hymenolobium excelsum. Every number below names the publication it came from.

PropertyAngelim-pedraPara-angelim
Janka hardness1,647 lbfLPF/SFB Madeiras Brasileiras1,720 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC50.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-947.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture17,181 lb/in²LPF/SFB Madeiras Brasileiras17,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.92 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.05 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength8,691 lb/in²LPF/SFB Madeiras Brasileiras8,990 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)13.5%LPF/SFB Madeiras Brasileiras10.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.67LPF/SFB Madeiras Brasileiras1.61USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.