Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Angelim-pedra vs Angelim-pedra

Hymenolobium pulcherrimum against Hymenolobium nitidum. Every number below names the publication it came from.

PropertyAngelim-pedraAngelim-pedra
Janka hardness1,206 lbfLPF/SFB Madeiras Brasileiras1,257 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC44.3 lb/ft³LPF/SFB Madeiras Brasileiras43.1 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture16,328 lb/in²LPF/SFB Madeiras Brasileiras13,683 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.81 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.68 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength9,088 lb/in²LPF/SFB Madeiras Brasileiras7,610 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)14.0%LPF/SFB Madeiras Brasileiras11.8%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.68LPF/SFB Madeiras Brasileiras1.66LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.