PropertyAnoerá-ferroCastanha-de-cutia
Janka hardness2,683 lbfLPF/SFB Madeiras Brasileiras2,696 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC60.6 lb/ft³LPF/SFB Madeiras Brasileiras64.9 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture20,326 lb/in²LPF/SFB Madeiras Brasileiras21,847 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.12 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.36 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength10,768 lb/in²LPF/SFB Madeiras Brasileiras11,748 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.1%LPF/SFB Madeiras Brasileiras17.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.82LPF/SFB Madeiras Brasileiras1.28LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.