Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Arapari vs Ararapari

Macrolobium acacifolium against Macrolobium sp. Every number below names the publication it came from.

PropertyArapariArarapari
Janka hardness1,153 lbfLPF/SFB Madeiras Brasileiras1,208 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC39.3 lb/ft³LPF/SFB Madeiras Brasileiras40.0 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture11,520 lb/in²LPF/SFB Madeiras Brasileiras11,961 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.29 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.44 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength6,202 lb/in²LPF/SFB Madeiras Brasileiras6,457 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)10.0%LPF/SFB Madeiras Brasileiras11.9%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.21LPF/SFB Madeiras Brasileiras2.37LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.