Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Atlantic white cedar vs Port-Orford cedar

Chamaecyparis thyoides against Chamaecyparis lawsoniana. Every number below names the publication it came from.

PropertyAtlantic white cedarPort-Orford cedar
Janka hardness350 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b630 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC22.3 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b30.1 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture6,800 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b12,700 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity0.93 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.70 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength4,700 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b6,250 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)8.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-310.1%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)1.86USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-31.50USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.