Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Australian Blackwood vs Black Wattle

Acacia melanoxylon against Acacia mollissima. Every number below names the publication it came from.

PropertyAustralian BlackwoodBlack Wattle
Janka hardness1,100 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)1,750 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC40.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)45.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture15,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)17,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.05 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.08 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength8,420 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)8,800 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)——
Tangential / radial ratio(lower is better)2.65Chudnoff 1984, Tropical Timbers of the World (AH-607)—

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.