Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Balsamo vs Canalete

Myroxylon balsamum against Cordia spp. (hard-wooded, dark-colored Gerascanthus group). Every number below names the publication it came from.

PropertyBalsamoCanalete
Janka hardness2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)58.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture20,130 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Modulus of elasticity2.43 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Crushing strength11,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Volumetric shrinkage(lower is better)10.0%Chudnoff 1984, Tropical Timbers of the World (AH-607)11.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.63Chudnoff 1984, Tropical Timbers of the World (AH-607)1.85Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.