PropertyBanakVirola
Janka hardness510 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1,041 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC36.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)38.0 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture10,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b13,825 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.04 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1.72 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength5,140 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b7,424 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.7%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-414.8%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.91USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-42.11LPF/SFB Madeiras Brasileiras

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.