Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Baracara vs Tento

Ormosia spp. against Ormosia coccinea. Every number below names the publication it came from.

PropertyBaracaraTento
Janka hardness1,000 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)1,378 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC44.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)44.9 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture17,860 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)13,725 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.34 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.44 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength9,780 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)7,253 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—10.9%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)—1.69LPF/SFB Madeiras Brasileiras

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.