Bitter Angelim vs Faveira-amargosa

Vatairea spp. against Vatairea guianensis. Every number below names the publication it came from.

PropertyBitter AngelimFaveira-amargosa
Janka hardness1,250 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)1,532 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC46.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)51.8 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture14,600 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)16,059 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.79 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.93 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength6,950 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)8,321 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)8.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)14.8%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.18Chudnoff 1984, Tropical Timbers of the World (AH-607)2.03LPF/SFB Madeiras Brasileiras

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.