PropertyBreuBreu-preto
Janka hardness2,317 lbfLPF/SFB Madeiras Brasileiras1,517 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC39.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)48.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture20,012 lb/in²LPF/SFB Madeiras Brasileiras16,556 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.25 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.83 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,449 lb/in²LPF/SFB Madeiras Brasileiras9,174 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.0%LPF/SFB Madeiras Brasileiras12.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.92LPF/SFB Madeiras Brasileiras2.00LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.