Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Brown-woolly fig vs Figueira / gameleira

Ficus drupacea against Ficus insipida. Every number below names the publication it came from.

PropertyBrown-woolly figFigueira / gameleira
Janka hardness369 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a269 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC24.3 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-928.1 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture—8,933 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity—1.15 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength—5,462 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—14.1%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)—1.94LPF/SFB Madeiras Brasileiras

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.