Caimito vs Canalete

Cynodendron spp- against Cordia spp. (hard-wooded, dark-colored Gerascanthus group). Every number below names the publication it came from.

PropertyCaimitoCanalete
Janka hardness2,530 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC59.6 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-958.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture——
Modulus of elasticity——
Crushing strength——
Volumetric shrinkage(lower is better)15.2%Chudnoff 1984, Tropical Timbers of the World (AH-607)11.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.34Chudnoff 1984, Tropical Timbers of the World (AH-607)1.85Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.