Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Cajuaçu vs Espave

Anacardium giganteum against Anacardium excelsum. Every number below names the publication it came from.

PropertyCajuaçuEspave
Janka hardness505 lbfLPF/SFB Madeiras Brasileiras470 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC30.6 lb/ft³LPF/SFB Madeiras Brasileiras30.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture9,303 lb/in²LPF/SFB Madeiras Brasileiras7,960 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.45 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.28 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength5,561 lb/in²LPF/SFB Madeiras Brasileiras4,530 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)8.5%LPF/SFB Madeiras Brasileiras—
Tangential / radial ratio(lower is better)2.21LPF/SFB Madeiras Brasileiras—

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.