Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Cajuaçu vs Cajuaçu

Anacardium occidentale = Anacardium microcarpum against Anacardium spruceanum. Every number below names the publication it came from.

PropertyCajuaçuCajuaçu
Janka hardness591 lbfLPF/SFB Madeiras Brasileiras560 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC28.7 lb/ft³LPF/SFB Madeiras Brasileiras31.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture8,079 lb/in²LPF/SFB Madeiras Brasileiras9,303 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.36 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.42 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength5,448 lb/in²LPF/SFB Madeiras Brasileiras5,291 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)9.7%LPF/SFB Madeiras Brasileiras9.4%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.74LPF/SFB Madeiras Brasileiras2.07LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.