Canela/louro-tamanco vs Canelo

Nectandra cuspidata against Nectandra spp.. Every number below names the publication it came from.

PropertyCanela/louro-tamancoCanelo
Janka hardness573 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,060 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC28.7 lb/ft³LPF/SFB Madeiras Brasileiras39.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture9,587 lb/in²LPF/SFB Madeiras Brasileiras14,230 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.24 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.65 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength5,462 lb/in²LPF/SFB Madeiras Brasileiras7,260 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)9.1%LPF/SFB Madeiras Brasileiras—
Tangential / radial ratio(lower is better)1.49LPF/SFB Madeiras Brasileiras—

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.