Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Canelo vs True mahogany

Nectandra spp. against Swietenia macrophylla. Every number below names the publication it came from.

PropertyCaneloTrue mahogany
Janka hardness1,060 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)800 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC39.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)41.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture14,230 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)11,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.65 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.50 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength7,260 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)6,780 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)—7.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)—1.37USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.