Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Capomo vs Amapá-doce

Brosimum spp. (Alicastrum group) against Brosimum parinarioides. Every number below names the publication it came from.

PropertyCapomoAmapá-doce
Janka hardness1,340 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)1,250 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC49.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-943.8 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture—14,834 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity—1.64 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength—8,264 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—12.6%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)—1.71LPF/SFB Madeiras Brasileiras

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.