Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Caucho vs Balsa

Castilla ulei against Ochroma pyramidale. Every number below names the publication it came from.

PropertyCauchoBalsa
Janka hardness313 lbfLPF/SFB Madeiras Brasileiras88 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC29.3 lb/ft³LPF/SFB Madeiras Brasileiras11.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture8,093 lb/in²LPF/SFB Madeiras Brasileiras3,140 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.29 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras0.49 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength5,333 lb/in²LPF/SFB Madeiras Brasileiras2,160 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)16.1%LPF/SFB Madeiras Brasileiras10.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.69LPF/SFB Madeiras Brasileiras2.53USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.