Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Cedar elm vs American elm

Ulmus crassifolia against Ulmus americana. Every number below names the publication it came from.

PropertyCedar elmAmerican elm
Janka hardness1,419 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a830 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC45.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-935.0 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture—11,800 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity—1.34 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength—5,520 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)15.4%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-314.6%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)2.17USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-32.26USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.