Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Chicha vs Axixá

Sterculia apetala against Sterculia apeibophylla. Every number below names the publication it came from.

PropertyChichaAxixá
Janka hardness400 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)686 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC25.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)38.1 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture7,110 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,218 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity0.96 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.52 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength4,230 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)6,685 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)11.8%Chudnoff 1984, Tropical Timbers of the World (AH-607)15.4%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.24Chudnoff 1984, Tropical Timbers of the World (AH-607)1.96LPF/SFB Madeiras Brasileiras

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.