Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Chupón vs Purpleheart

Pradosia spp. against Peltogyne spp.. Every number below names the publication it came from.

PropertyChupónPurpleheart
Janka hardness1,880 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)1,860 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC52.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture17,770 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)19,200 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity2.32 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.27 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength7,660 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)10,320 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)14.8%Chudnoff 1984, Tropical Timbers of the World (AH-607)9.9%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)2.39Chudnoff 1984, Tropical Timbers of the World (AH-607)1.91USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.