Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Conduru / pau-vermelho vs Janitá

Brosimum rubescens against Brosimum alicastrum. Every number below names the publication it came from.

PropertyConduru / pau-vermelhoJanitá
Janka hardness2,062 lbfLPF/SFB Madeiras Brasileiras2,059 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC50.6 lb/ft³LPF/SFB Madeiras Brasileiras58.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture20,609 lb/in²LPF/SFB Madeiras Brasileiras22,146 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.25 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.32 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength10,724 lb/in²LPF/SFB Madeiras Brasileiras12,502 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.2%LPF/SFB Madeiras Brasileiras16.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.47LPF/SFB Madeiras Brasileiras1.68LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.