Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Cuangare vs Spanish-cedar

Dialyanthera spp. against Cedrela spp.. Every number below names the publication it came from.

PropertyCuangareSpanish-cedar
Janka hardness380 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b600 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC28.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)35.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture7,300 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b11,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.52 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1.44 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength4,760 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b6,210 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)12.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-410.3%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)2.24USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.50USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.