Custard apple vs Embira

Annona reticulata against Annona exsucca = Rollinia exsucca. Every number below names the publication it came from.

PropertyCustard appleEmbira
Janka hardness791 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a864 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC34.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-939.6 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture—13,000 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity—1.71 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength—7,581 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—12.3%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)—2.75LPF/SFB Madeiras Brasileiras

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.