Duru vs Pau-de-jangada

Apeiba spp. against Apeiba echinata. Every number below names the publication it came from.

PropertyDuruPau-de-jangada
Janka hardness250 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)558 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC14.0 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-926.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture4,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)7,667 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity—0.97 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength670 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)4,608 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)7.8%Chudnoff 1984, Tropical Timbers of the World (AH-607)9.3%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)3.00Chudnoff 1984, Tropical Timbers of the World (AH-607)2.83LPF/SFB Madeiras Brasileiras

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.