Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

East African Satinwood vs Panga Panga

Pagara macrophylla against Millettia spp.. Every number below names the publication it came from.

PropertyEast African SatinwoodPanga Panga
Janka hardness2,064 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,630 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC53.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture15,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)16,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.99 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.97 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength8,020 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)9,950 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)——
Tangential / radial ratio(lower is better)—1.87Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.