Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Embira-preta vs Embira-preta

Guatteria olivacea against Guatteria procera. Every number below names the publication it came from.

PropertyEmbira-pretaEmbira-preta
Janka hardness883 lbfLPF/SFB Madeiras Brasileiras1,468 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC53.1 lb/ft³LPF/SFB Madeiras Brasileiras50.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture13,668 lb/in²LPF/SFB Madeiras Brasileiras17,622 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.66 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.22 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength6,792 lb/in²LPF/SFB Madeiras Brasileiras10,028 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.0%LPF/SFB Madeiras Brasileiras18.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.11LPF/SFB Madeiras Brasileiras1.58LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.