Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Eveuss vs Ipe

Klainedoxa gabonensis against Tabebuia spp., lapacho group. Every number below names the publication it came from.

PropertyEveussIpe
Janka hardness3,647 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a3,680 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC68.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)70.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture26,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)25,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity3.52 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)3.14 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength13,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)13,010 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)16.0%Chudnoff 1984, Tropical Timbers of the World (AH-607)13.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.52Chudnoff 1984, Tropical Timbers of the World (AH-607)1.21USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.