Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Faveira-amargosa vs Bitter Angelim

Vatairea guianensis against Vatairea spp.. Every number below names the publication it came from.

PropertyFaveira-amargosaBitter Angelim
Janka hardness1,532 lbfLPF/SFB Madeiras Brasileiras1,250 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC51.8 lb/ft³LPF/SFB Madeiras Brasileiras46.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture16,059 lb/in²LPF/SFB Madeiras Brasileiras14,600 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.93 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.79 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength8,321 lb/in²LPF/SFB Madeiras Brasileiras6,950 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)14.8%LPF/SFB Madeiras Brasileiras8.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)2.03LPF/SFB Madeiras Brasileiras2.18Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.