Vataireopsis speciosa against Swietenia macrophylla. Every number below names the publication it came from.

PropertyFaveira-amargosaTrue mahogany
Janka hardness1,043 lbfLPF/SFB Madeiras Brasileiras800 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC46.2 lb/ft³LPF/SFB Madeiras Brasileiras41.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture14,749 lb/in²LPF/SFB Madeiras Brasileiras11,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.68 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.50 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength7,694 lb/in²LPF/SFB Madeiras Brasileiras6,780 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)9.9%LPF/SFB Madeiras Brasileiras7.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)2.12LPF/SFB Madeiras Brasileiras1.37USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.