Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Faveira / visgueiro vs Faveira

Parkia paraensis against Parkia multijuga. Every number below names the publication it came from.

PropertyFaveira / visgueiroFaveira
Janka hardness743 lbfLPF/SFB Madeiras Brasileiras668 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC33.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-928.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture10,668 lb/in²LPF/SFB Madeiras Brasileiras8,791 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.66 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.25 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength5,604 lb/in²LPF/SFB Madeiras Brasileiras5,362 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)11.9%LPF/SFB Madeiras Brasileiras9.8%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.17LPF/SFB Madeiras Brasileiras2.41LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.