PropertyFiddlewoodMolave
Janka hardness1,160 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)1,255 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC43.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)50.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture12,890 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)17,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.57 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.00 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength7,010 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)9,400 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)10.4%Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Tangential / radial ratio(lower is better)2.00Chudnoff 1984, Tropical Timbers of the World (AH-607)1.44Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.