Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Figueira / gameleira vs Balsa

Ficus insipida against Ochroma pyramidale. Every number below names the publication it came from.

PropertyFigueira / gameleiraBalsa
Janka hardness269 lbfLPF/SFB Madeiras Brasileiras88 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC28.1 lb/ft³LPF/SFB Madeiras Brasileiras11.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture8,933 lb/in²LPF/SFB Madeiras Brasileiras3,140 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.15 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras0.49 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength5,462 lb/in²LPF/SFB Madeiras Brasileiras2,160 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)14.1%LPF/SFB Madeiras Brasileiras10.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.94LPF/SFB Madeiras Brasileiras2.53USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.