Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Five-stamen tamarisk vs Southern red oak

Tamarix chinensis against Quercus falcata. Every number below names the publication it came from.

PropertyFive-stamen tamariskSouthern red oak
Janka hardness1,054 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,060 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC39.6 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-941.3 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture—10,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity—1.49 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength—6,090 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)—16.1%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)—2.40USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.