Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Freijó vs Canalete

Cordia goeldiana against Cordia spp. (hard-wooded, dark-colored Gerascanthus group). Every number below names the publication it came from.

PropertyFreijóCanalete
Janka hardness996 lbfLPF/SFB Madeiras Brasileiras2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC36.3 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-958.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture13,256 lb/in²LPF/SFB Madeiras Brasileiras—
Modulus of elasticity1.48 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras—
Crushing strength7,353 lb/in²LPF/SFB Madeiras Brasileiras—
Volumetric shrinkage(lower is better)10.6%LPF/SFB Madeiras Brasileiras11.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.61LPF/SFB Madeiras Brasileiras1.85Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.