Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Garrote vs Mururé

Brosimum sp against Brosimum acutifolium subsp interjectum. Every number below names the publication it came from.

PropertyGarroteMururé
Janka hardness1,074 lbfLPF/SFB Madeiras Brasileiras1,120 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC36.2 lb/ft³LPF/SFB Madeiras Brasileiras42.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture13,526 lb/in²LPF/SFB Madeiras Brasileiras14,508 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.69 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.69 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength7,467 lb/in²LPF/SFB Madeiras Brasileiras7,922 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)0.7%LPF/SFB Madeiras Brasileiras12.6%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.40LPF/SFB Madeiras Brasileiras1.63LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.