PropertyGmelinaTeak
Janka hardness622 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)1,000 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC30.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)40.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture8,650 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)14,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity0.80 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.55 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength4,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)8,410 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)8.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-47.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)2.04USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-42.32USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.