Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Gogó-de-guariba vs White oak

Rauvolfia paraensis against Quercus alba. Every number below names the publication it came from.

PropertyGogó-de-guaribaWhite oak
Janka hardness1,203 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,360 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC44.3 lb/ft³LPF/SFB Madeiras Brasileiras47.6 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture16,144 lb/in²LPF/SFB Madeiras Brasileiras15,200 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.82 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.78 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength8,292 lb/in²LPF/SFB Madeiras Brasileiras7,440 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)13.3%LPF/SFB Madeiras Brasileiras16.3%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)1.93LPF/SFB Madeiras Brasileiras1.88USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.