Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Goiabão vs Maçarandubarana

Chrysophyllum lucentifolium = Pouteria pachycarpa against Chrysophyllum prieurii. Every number below names the publication it came from.

PropertyGoiabãoMaçarandubarana
Janka hardness2,646 lbfLPF/SFB Madeiras Brasileiras2,725 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC58.1 lb/ft³LPF/SFB Madeiras Brasileiras61.8 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture22,999 lb/in²LPF/SFB Madeiras Brasileiras25,232 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.41 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.49 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,357 lb/in²LPF/SFB Madeiras Brasileiras10,810 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)16.5%LPF/SFB Madeiras Brasileiras20.3%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.81LPF/SFB Madeiras Brasileiras1.69LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.