PropertyGolden showerCanafístula
Janka hardness2,139 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a2,500 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC55.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-954.3 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture—16,527 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity—1.91 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength—10,469 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)——
Tangential / radial ratio(lower is better)—1.47LPF/SFB Madeiras Brasileiras

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.