Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Grand fir vs Noble fir

Abies grandis against Abies procera. Every number below names the publication it came from.

PropertyGrand firNoble fir
Janka hardness490 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b410 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC25.8 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b27.3 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture8,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b10,700 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.57 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.72 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength5,290 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b6,100 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)11.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-312.4%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)2.21USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-31.93USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.