Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Guarea vs Cramantee

Guarea cedrata against Guarea spp.. Every number below names the publication it came from.

PropertyGuareaCramantee
Janka hardness1,000 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)1,065 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC36.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)39.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture14,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)11,400 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.37 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.60 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength7,720 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)6,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)—11.2%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)—2.06Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons