PropertyHayaAndaman Padauk
Janka hardness1,725 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,630 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC49.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-948.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture——
Modulus of elasticity——
Crushing strength——
Volumetric shrinkage(lower is better)—6.4%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)—1.33Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.