PropertyHoneylocustCherrybark oak
Janka hardness1,580 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1,480 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC46.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-947.6 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture14,700 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b18,100 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.63 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b2.28 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength7,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b8,740 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)10.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3—
Tangential / radial ratio(lower is better)1.57USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3—

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • manual map (regional variant)public domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA FIA REF_SPECIESpublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.