PropertyHuraSpanish-cedar
Janka hardness550 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b600 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC30.0 lb/ft³LPF/SFB Madeiras Brasileiras35.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture8,700 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b11,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.17 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b1.44 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength4,800 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b6,210 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)7.3%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-410.3%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.67USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.50USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.