Ilomba vs Obeche

Pycnanthus angolensis against Triplochiton scleroxylon. Every number below names the publication it came from.

PropertyIlombaObeche
Janka hardness610 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b430 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC29.8 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-924.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture9,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b7,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.59 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b0.86 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength5,550 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b3,930 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)12.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-49.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.83USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.80USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.