Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Indian Almond Wood vs White Bombay

Terminalia catappa against Terminalia procera. Every number below names the publication it came from.

PropertyIndian Almond WoodWhite Bombay
Janka hardness1,030 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,070 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC40.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)40.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture——
Modulus of elasticity——
Crushing strength——
Volumetric shrinkage(lower is better)10.3%Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Tangential / radial ratio(lower is better)1.27Chudnoff 1984, Tropical Timbers of the World (AH-607)—

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.